The effect of five kinds of surface treatment agents on the bond strength to various ceramics with thermocycle aging
Yukari NODAMasatoshi NAKAJIMAMasahiro TAKAHASHITeerapong MAMANEEKeiichi HOSAKATomohiro TAKAGAKIMasaomi IKEDARichard M. FOXTONJunji TAGAMI
Author information
JOURNAL FREE ACCESS

2017 Volume 36 Issue 6 Pages 755-761

Details
Abstract

This study evaluated the effects of ceramic surface treatment agents on shear bond strengths to ceramic materials with and without thermocycling. Ceramic plates were prepared from feldspathic ceramic; AAA, lithium disilicate ceramic material; IPS e.max Press, zirconia ceramic; Lava. Ceramic surfaces were pretreated with one of five surface treatment agents (Clearfil PhotoBond mixed with Porcelainbond activator (PB), Clearfil SE One mixed with Porcelainbond activator (SO), Ceramic Primer (CP), Universal Primer (UP), Scotchbond Universal (SU)), and then a resin cement (Clapearl DC) was filled. After 0, 5,000, and 10,000 thermocycles, micro-shear bond strengths between ceramic-cement interfaces were determined. SU exhibited significantly lower initial bond strength to AAA and e.max than PB, SO, CP, and UP. For Lava, PB, SO, CP and SU exhibited higher initial bond strengths than UP. Thermocycles reduced bond strengths to all the ceramic materials with any surface treatment.

Content from these authors
© 2017 The Japanese Society for Dental Materials and Devices
Previous article Next article
feedback
Top