Abstract:

The run-of-mine ore samples which have been used in the study were taken from a fluorite ore. The grade of fluorite was 28.65%. From the condition test, the optimal grinding fineness was-0.074mm accounted for 79.5%. The final optimal reagent system was A1B3C3D3E3 with comprehensive consideration. That is, sodium carbonate was 2000 g/t, sodium silicate was 1000 g/t, aluminum sulfate was 200 g/t, sodium hexametaphosphate usage was 1000 g/t, oleic acid dosage for 2000 g/t. Through the closed-circuit test of flotation, the final index was the fluorite grade of the concentrate was 97.69% and the recovery was 48.07%.

You might also be interested in these eBooks

Info:

Periodical:

Advanced Materials Research (Volumes 734-737)

Pages:

1068-1072

Citation:

Online since:

August 2013

Export:

Price:

[1] SHEN ZhangFeng, DING Xing, REN QianQian. Technological Innovations for Separation and Refinement of Fluorite Mineral, J. 95(2012) 68-70.

Google Scholar

[2] Huang Guozhi, Gan Jingchao. Present situation and practice of research on fluorite flotation, J. 4(1995) 37-44.

Google Scholar

[3] NIU Fangyin, ZHANG Qin, ZHANG Jie. Orthogonal Test Research On Flotation Desulfurization of High-Sulfur Bauxite, J. 27(2007) 393-395.

Google Scholar